The Reasons For PE Pipe Surface Appears Pits Or Bubbles And Settle Method

Aug 02, 2018

Appearance this problem, mainly because raw material is not good, maybe there are other things in it, or moisture; If there are other things in the raw materials, we have to change it or sieve it. If the raw material moisture, we dry it. If you have any questions about bubbles on the PE pipe surface, welcome to contact us.